Cross-section shape
Features
•Static antistatic performance
•Low particle level
•Low ion contamination
•Both sides of spacer have the same surface pattern
Specification
Model number | PEA-□-350(Z1) (□:diameter) |
|
---|---|---|
Material | Conductive PE | |
Surface Resistance |
R < 10^11Ω | |
Emboss Thickness | 350μm |
Carton size
Model number | Carton size W×L×H (mm) |
Quantity (sheet) |
G/W (kg) |
Corresponding container |
---|---|---|---|---|
PEA-4-350 (Z1) | 435×230×185 | 4,000 | 3.7 | MA-4 |
PEA-5-350 (Z1) | 280×150×270 | 2,000 | 2.5 | MA-5 |
PEA-6-350(Z1) | 330×180×240 | 2,000 | 3.7 | MA-6S |
PEA-8-350(Z1) | 440×230×250 | 2,000 | 6.6 | MA-8S |
PEA-9-350(Z1) | 255×255×205 | 1,000 | 4.5 | ND-6N |
PEA-295-350(Z1) | 340×340×170 | 500 | 3.8 | ND-8 |
PEA-12-350(Z1) | 640×335×160 | 1,000 | 7.8 | NA-300LA |
PEA-15.5-350(Z1) | 435×435×195 | 500 | 7.0 | NDM-12 |
Physical property data
Item | Data |
---|---|
Resistance(23°C 60%RH) | 2.0 × 10^9 Ω |
Charging potential | 7-12 V |
Decay time (1kV→100V) |
8-13 sec |
Particle APC(0.5μm<) | 24 counts/pc |
Ion contamination 【anion】(ppb) | Cl:3 NO3:1 SO4:ND |
Ion contamination 【cation】(ppb) | Na:1 K:260 |
* This data is an actual measurement value, not a uaranteed value.
Comparison data with competitors
Item | PEA(Z1) | Dust-free paper | Woven fabric |
---|---|---|---|
Resistance | good | bad | bad |
Charging potential | good | bad | bad |
Decay Time | bad | bad | bad |
Particle APC |
good | bad | bad |
Ion contamination | good | bad | bad |
Resistance comparison
Sample | PEA (Z1) | Dust-free paper | Woven fabric | |
---|---|---|---|---|
Measurement environment |
23°C 15%RH |
9.20×10^10 | 1.0×10^13< | 1.0×10^13< |
23°C 30%RH |
7.70×10^10 | 3.20×10^11 | 1.0×10^13< | |
23°C 60%RH |
2.00×10^9 | 3 80×10^9 | 1.0×10^13< | |
23°C 95%RH |
9.30×10^8 | 3.40×10^6 | 1.0×10^13< |
※Unit : Ω
* This data is an actual measurement value, not a uaranteed value.
Charging potential, decay time comparison
Sample | PEA(Z1) | Dust-free paper | Woven fabric | |
---|---|---|---|---|
Charging potential (V) |
0-1 | 2000< | 2000< | |
Decay Time(sec) | +1kv→+100V | <0.1 | 12-100< | 100< |
-1kv→-100V | <0.1 | 10-100< | 100< |
* This data is an actual measurement value, not a guaranteed value.
Particle comparison APC
Sample (size. 8inch) |
PEA(Z1) | Dust-free paper | Woven fabric |
---|---|---|---|
0.3um≦ | 31 | 507.7 | 204 |
0.5um≦ | 23.8 | 328.3 | 128.3 |
1um≦ | 10.6 | 181.3 | 68 |
3um≦ | 5.6 | 93.7 | 28.7 |
5um≦ | 5.4 | 81,7 | 21.7 |
10um≦ | 2.6 | 41 | 6.3 |
30um≦ | 0.4 | 4 | 2.7 |
50um≦ | 0.2 | 1.8 | 1.4 |
* This data is an actual measurement value, not a guaranteed value.
Ion contamination comparison
Sample | Anion | ||||||
---|---|---|---|---|---|---|---|
F | Cl | NO2 | Br | NO3 | SO4 | PO4 | |
PEA (Z1) | ND | 3 | ND | ND | 1 | ND | ND |
Dust-free paper | ND | 540 | ND | ND | 52 | 830 | 4 |
Woven fabric | ND | 2 | ND | ND | 1 | ND | ND |
Sample | Cation | ||||||
Li | Na | NH4 | K | Mg | Ca | ||
PEA (Z1) | ND | 1 | ND | 260 | ND | ND | |
Dust-free paper | ND | 300 | ND | 970 | ND | ND | |
Woven fabric | ND | ND | 1 | ND | ND | ND |
※Unit : ppb(μg /l)
* This data is an actual measurement value, not a uaranteed value.
Outgassing comparison
Sample | PEA(Z1) | Dust-free paper | Woven fabric |
---|---|---|---|
Total outgassing | 0.22 | 0.005 | 0.142 |
BHT | ND | 0.0003 | ND |
* This data is an actual measurement value, not a guaranteed value.